Electronic Manufacturing Services · Dorval, Québec · Established 1993
Home/Lead-free vs leaded solder
Guide

Lead-Free vs Leaded Solder: Which Should You Use?

Lead-free (SAC) vs tin-lead solder explained: melting points, RoHS requirements and exemptions, reliability, appearance, mixing finishes and how to choose for your PCB assembly.

Quick answer

Most products sold in markets with RoHS-type rules must use lead-free solder, typically a tin-silver-copper (SAC) alloy that melts around 217–220 °C, compared with 183 °C for traditional 63/37 tin-lead. Leaded solder is still used where products are exempt or out of scope, often for certain high-reliability applications. The choice should follow your compliance requirements first, then reliability needs.

The two families

Tin-lead (e.g. 63/37)Lead-free (e.g. SAC305)
Main metalsTin and leadTin, silver and copper
Melting pointAbout 183 °C (eutectic)About 217–220 °C
Reflow temperaturesLowerHigher — more thermal stress on parts and boards
RoHS compliantNoYes
Joint appearanceBright and smoothDuller and grainier — normal for lead-free
Typical use todayExempt or out-of-scope products, some high-reliability workMost commercial and industrial products

What RoHS requires

RoHS (Restriction of Hazardous Substances) limits lead and other substances in electrical and electronic equipment. In practice, most products sold in the EU — and many sold elsewhere because of customer requirements — must be built lead-free.

Some product categories are outside the scope of RoHS or covered by specific exemptions, and some high-reliability programs still specify tin-lead. Check the current regulation and your customer’s requirements rather than assuming either way.

Reliability differences

  • Lead-free alloys are stiffer; behaviour under thermal cycling, vibration and drop differs from tin-lead and depends on the application
  • Higher reflow temperatures increase stress on components, laminates and moisture-sensitive parts — choose materials rated for lead-free processing
  • Pure-tin finishes can grow tin whiskers over time, a concern for some long-life, high-reliability products
  • Both can be reliable when the design, materials and process are matched to the application

Don’t mix without a plan

Problems often come from mixing: lead-free BGA balls reflowed with tin-lead paste, or components and finishes that don’t match the process. Mixed assemblies need a deliberate process and profile. State clearly on your documentation whether the build is lead-free or leaded.

💡 Lead-free joints look duller than tin-lead joints. That’s normal and accepted by IPC-A-610 — it doesn’t mean the joint is cold or defective.

How to choose

  • Required to be RoHS compliant? Use lead-free
  • Exempt or out of scope, and your program specifies tin-lead? Leaded can be used
  • Unsure? Check the regulation that applies to your market and ask your customer
  • Make sure the components, board finish and laminate all suit the chosen process

At JLS

JLS solders both RoHS (lead-free) and non-RoHS (leaded) assemblies, with aqueous or no-clean chemistry, and our materials are RoHS and REACH compliant. Tell us which process your product requires in your quote request.

Ready to send your project?

Send your files or describe your project. An engineer reviews every request, and most quotes go out within 48 hours.

Get a quote →
FAQ

Frequently asked questions

What is the melting point of lead-free solder?

Common SAC lead-free alloys such as SAC305 melt at about 217–220 °C, compared with about 183 °C for eutectic 63/37 tin-lead solder.

Is leaded solder still allowed?

For products in RoHS scope, generally no. Some product categories are out of scope or exempt, and some programs still specify tin-lead. Check the regulation that applies to your product.

Is lead-free solder less reliable?

Not inherently. It behaves differently, and its reliability depends on the application, materials and process. Many high-reliability products are built lead-free.

Why do lead-free solder joints look dull?

Lead-free alloys naturally solidify with a duller, grainier surface. This is normal and acceptable under IPC-A-610.

Can JLS build both lead-free and leaded assemblies?

Yes. We solder RoHS (lead-free) and non-RoHS (leaded) assemblies, with aqueous or no-clean chemistry.