Moisture-Sensitive Devices: What MSL Means for Your Assembly

What moisture sensitivity levels (MSL 1–6) mean, floor life, dry packing, baking and why moisture-sensitive components crack or delaminate during reflow.

Quick answer

Many plastic IC packages absorb moisture from the air. During reflow that moisture turns to steam and can crack or delaminate the package. The moisture sensitivity level (MSL), from 1 to 6, tells how long a part can sit out of its sealed dry pack before it must be soldered or baked. Correct storage, tracking and baking prevent these hidden failures.

MSL levels and floor life

LevelTypical floor life out of dry pack (at ≤30 °C / 60 % RH)
MSL 1Unlimited
MSL 21 year
MSL 2a4 weeks
MSL 3168 hours
MSL 472 hours
MSL 548 hours
MSL 5a24 hours
MSL 6Must be baked before use; time limit on label
💡 These are the standard values from the IPC/JEDEC moisture-sensitivity standards. The part’s label and datasheet are the final reference.

What goes wrong

If a moisture-loaded part is reflowed, the rapid heating turns trapped moisture into steam. The result can be internal delamination, cracks (sometimes called popcorning) or damaged bond wires — defects that may not be visible and can fail later in the field.

Good handling practice

  • Keep parts in their sealed moisture-barrier bags with desiccant and humidity indicator cards until needed
  • Track how long each opened reel or tray has been exposed
  • Reseal or store opened parts in dry storage
  • Bake parts that exceeded their floor life, following the manufacturer’s guidance
  • For consigned parts, ship them sealed — don’t open bags to count parts

At JLS

In a turnkey order, JLS sources your components through a managed, traceable supply chain, so moisture-sensitive parts arrive in their original packaging. If you supply some parts yourself, send moisture-sensitive components in their sealed bags and mention it in your quote request.

Ready to send your project?

Send your files or describe your project. An engineer reviews every request, and most quotes go out within 48 hours.

Get a quote →
FAQ

Frequently asked questions

What does MSL 3 mean?

An MSL 3 part can typically be out of its dry pack for up to 168 hours (one week) at up to 30 °C and 60 % relative humidity before it must be soldered or baked.

What happens if moisture-sensitive parts aren’t handled correctly?

Moisture can turn to steam during reflow and crack or delaminate the package, causing failures that may only appear later.

Can an exposed part still be used?

Usually yes, after baking according to the manufacturer’s guidance, which drives out the absorbed moisture.

How should I ship consigned moisture-sensitive parts?

In their original sealed moisture-barrier bags with desiccant and humidity indicator cards — don’t open them to count.